SLIMATIC MORTAR MOULDING DEMO PRESENTATION SLIMATIC MORTAR MOULDING PROPERTIES The 10 to 12 seconds time required to tamp 32 times in 4 rounds is always respected. – PowerPoint PPT presentation

Number of Views:42
Avg rating:3.0/5.0
Slides: 4
Provided by: SergeVa1
Category:

less

Transcript and Presenter's Notes

Title: SLIMATIC MORTAR MOULDING


1
SLIMATIC MORTAR MOULDING
  • DEMO
  • PRESENTATION

2
SLIMATIC MORTAR MOULDINGPROPERTIES
  • The 10 to 12 seconds time required to tamp 32
    times in 4 rounds is always respected.
  • Respects the 2 minutes and 30 secondes after
    completion of the original mixing of the mortar
    batch.
  • Respects the tamping sequence.

3
SLIMATIC MORTAR MOULDINGPROPERTIES
  • Three cube compartments prepared at the same time
    (equivalent to three hands).